Ultrafast Emergence of Ferromagnetism in Antiferromagnetic FeRh in High Magnetic Fields
Authors:
I. A. Dolgikh,
T. G. H. Blank,
A. G. Buzdakov,
G. Li,
K. H. Prabhakara,
S. K. K. Patel,
R. Medapalli,
E. E. Fullerton,
O. V. Koplak,
J. H. Mentink,
K. A. Zvezdin,
A. K. Zvezdin,
P. C. M. Christianen,
A. V. Kimel
Abstract:
Ultrafast heating of FeRh by a femtosecond laser pulse launches a magneto-structural phase transition from an antiferromagnetic to a ferromagnetic state. Aiming to reveal the ultrafast kinetics of this transition, we studied magnetization dynamics with the help of the magneto-optical Kerr effect in a broad range of temperatures (from 4 K to 400 K) and magnetic fields (up to 25 T). Three different…
▽ More
Ultrafast heating of FeRh by a femtosecond laser pulse launches a magneto-structural phase transition from an antiferromagnetic to a ferromagnetic state. Aiming to reveal the ultrafast kinetics of this transition, we studied magnetization dynamics with the help of the magneto-optical Kerr effect in a broad range of temperatures (from 4 K to 400 K) and magnetic fields (up to 25 T). Three different types of ultrafast magnetization dynamics were observed and, using a numerically calculated H-T phase diagram, the differences were explained by different initial states of FeRh corresponding to a (i) collinear antiferromagnetic, (ii) canted antiferromagnetic and (iii) ferromagnetic alignment of spins. We argue that ultrafast heating of FeRh in the canted antiferromagnetic phase launches practically the fastest possible emergence of magnetization in this material. The magnetization emerges on a time scale of 2 ps, which corresponds to the earlier reported time-scale of the structural changes during the phase transition.
△ Less
Submitted 27 July, 2023; v1 submitted 8 February, 2022;
originally announced February 2022.
New single-molecule magnet based on Mn12 oxocarboxylate clusters with mixed carboxylate ligands, [Mn12O12(CN-o-C6H4CO2)12(CH3CO2)4(H2O)4]*8CH2Cl2: synthesis, crystal and electronic structure, magnetic properties
Authors:
Lyudmila A. Kushch,
Valentina D. Sasnovskaya,
Alexey I. Dmitriev,
Eduard B. Yagubskii,
Oksana V. Koplak,
Leokadiya V. Zorina,
Danil W. Boukhvalov
Abstract:
A new high symmetry Mn12 oxocarboxylate cluster [Mn12O12(CN-o-C6H4CO2)12(CH3CO2)4(H2O)4]*8CH2Cl2 (1) with mixed carboxylate ligands is reported. It was synthesized by the standard carboxylate substitution method. 1 crystallizes in the tetragonal space group I41/a. Complex 1 contains a [Mn12O12] core with eight CN-o-C6H4CO2 ligands in the axial positions, four CH3CO2 and four CN-o-C6H4CO2 those in…
▽ More
A new high symmetry Mn12 oxocarboxylate cluster [Mn12O12(CN-o-C6H4CO2)12(CH3CO2)4(H2O)4]*8CH2Cl2 (1) with mixed carboxylate ligands is reported. It was synthesized by the standard carboxylate substitution method. 1 crystallizes in the tetragonal space group I41/a. Complex 1 contains a [Mn12O12] core with eight CN-o-C6H4CO2 ligands in the axial positions, four CH3CO2 and four CN-o-C6H4CO2 those in equatorial positions. Four H2O molecules are bonded to four Mn atoms in an alternating up, down, up, down arrangement indicating 1:1:1:1 isomer. The Mn12 molecules in 1 are self-assembled by complementary hydrogen C-H...N bonds formed with participation of the axial o-cyanobenzoate ligands of the adjacent Mn12 clusters. The lattice solvent molecules (CH2Cl2) are weakly interacted with Mn12 units that results in solvent loss immediately after removal of the crystals from the mother liquor. The electronic structure and the intramolecular exchange parameters have been calculated. Mn 3d bands of 1 are rather broad and center of gravity of the bands shifts down from Fermi level. The overlap between Mn 3d bands and 2p ones of the oxygen atoms from carboxylate bridges is higher than in the parent Mn12-acetate cluster. These changes in electronic structure provide significant difference in the exchange interactions in comparison to Mn12-acetate. The magnetic properties have been studied on a dried (solvent-free) polycrystalline sample of 1. The dc magnetic susceptibility measurements in the 2-300 K temperature range support a high-spin ground state (S = 10).
△ Less
Submitted 26 September, 2012;
originally announced September 2012.