Ultra-Low Temperature Li/CFx Batteries Enabled by Fast-transport and Anion-pairing Liquefied Gas Electrolytes
Authors:
Yijie Yin,
John Holoubek,
Alex Liu,
Baharak Sayahpour,
Ganesh Raghavendran,
Guorui Cai,
Bing Han,
Matthew Mayer,
Noah B. Schorr,
Timothy N. Lambert,
Katharine L. Harrison,
Weikang Li,
Zheng Chen,
Y. Shirley Meng
Abstract:
Lithium fluorinated carbon is one of the most promising chemistries for high-energy-density primary energy storage systems in applications where rechargeability is not required. Though Li/CFx demonstrates high energy density under ambient conditions, achieving such a high energy density when exposed to subzero temperatures remains a challenge, particularly under high current density. Here, we repo…
▽ More
Lithium fluorinated carbon is one of the most promising chemistries for high-energy-density primary energy storage systems in applications where rechargeability is not required. Though Li/CFx demonstrates high energy density under ambient conditions, achieving such a high energy density when exposed to subzero temperatures remains a challenge, particularly under high current density. Here, we report a liquefied gas electrolyte with an anion-pair solvation structure based on dimethyl ether with a low melting point and low viscosity, leading to high ionic conductivity between a wide temperature range. Besides that, through systematic X-ray photoelectron spectroscopy integrated with transmission electron microscopy characterizations, we evaluate the interface of CFx for low-temperature performance. We conclude that the fast transport and anion-pairing solvation structure of the electrolyte bring about reduced charge transfer resistance at low temperatures, which resulted in significantly enhanced performance of Li/CFx cells. Utilizing 50 mg/cm2 loading electrodes, the Li/CFx still displayed 1530 Wh/kg at reduced temperature. This work provides insights into the electrolyte design that may overcome the operational limits of batteries in extreme environments.
△ Less
Submitted 1 September, 2022;
originally announced September 2022.
-
Galvanic Corrosion and Electric Field in Lithium Anode Passivation Films: Effects on Self-Discharge
Authors:
Kevin Leung,
Laura C. Merrill,
Katharine L. Harrison
Abstract:
Battery interfaces help govern rate capability, safety/stability, cycle life, and self-discharge, but significant gaps remain in our understanding at atomic length scales that can be exploited to improve interfacial properties. In particular, Li partially plated on copper current collectors, relevant to the anodeless, lithium metal cell which is a holy grail of high density energy battery research…
▽ More
Battery interfaces help govern rate capability, safety/stability, cycle life, and self-discharge, but significant gaps remain in our understanding at atomic length scales that can be exploited to improve interfacial properties. In particular, Li partially plated on copper current collectors, relevant to the anodeless, lithium metal cell which is a holy grail of high density energy battery research, has recently been reported to undergo galvanic corrosion and exhibit short shelf lives. We apply large scale Density Functional Theory (DFT) calculations and X-ray photoelectron spectroscopy to examine the reaction between the electrolyte and Li|Cu junctions coated with thin, uniform electrolyte interphase (SEI) passivating films at two applied voltages. These novel DFT galvanic corrosion simulations show that electrolyte degradation preferentially occurs on Li-plated regions and should lead to thicker SEI films. Our simulations reveal similarities but also fundamental differences between traditional metal localized pitting and Li-corrosion mechanisms. Furthermore, using the recently proposed, highly reactive lithium hydride (LiH) component SEI as example, we distinguish between electrochemical and chemical degradation pathways which are partially responsible for self-discharge, with the chemical pathway found to exhibit slow kinetics. We also predict that electric fields should in general exist across natural SEI components like LiH, and across artificial SEI films like LiI and LiAlO(2) often applied to improve battery cycling. Underlying and unifying these predictions is a framework of DFT voltage/overpotential definitions which we have derived from electrochemistry disciplines like structural metal corrosion studies; our analysis can only be made using the correct electronic voltage definitions.
△ Less
Submitted 23 May, 2022;
originally announced May 2022.
-
Edge-Propagation Discharge Mechanism in CFx Batteries -- a First Principles and Experimental Study
Authors:
Kevin Leung,
Noah B. Schorr,
Matthew Mayer,
Timothy N. Lambert,
Y. Shirley Meng,
K. L. Harrison
Abstract:
Graphite fluoride (CFx) cathodes coupled with lithium anodes yield one of the highest theoretical energy densities (>860 Wh/g) among primary batteries. In practice, the observed discharge voltage (~2.5 V) is significantly lower than thermodynamic limits (>4.5 V), the discharge rate is low, and so far Li/CFx has only been used in primary batteries. Understanding the discharge mechanism at atomic le…
▽ More
Graphite fluoride (CFx) cathodes coupled with lithium anodes yield one of the highest theoretical energy densities (>860 Wh/g) among primary batteries. In practice, the observed discharge voltage (~2.5 V) is significantly lower than thermodynamic limits (>4.5 V), the discharge rate is low, and so far Li/CFx has only been used in primary batteries. Understanding the discharge mechanism at atomic length scales will improve practical CFx energy density, rate capability, and rechargeability. So far, purely experimental techniques have not identified the correct discharge mechanism or explained the discharge voltage. We apply Density Functional Theory calculations to demonstrate that a CFx-edge propagation discharge mechanism based on lithium insertion at the CF/C boundary in partially discharged CFx exhibits a voltage range of 2.5 to 2.9 V -- depending on whether solvent molecules are involved. The voltages and solvent dependence agrees with our discharge and galvanostatic intermittent titration technique measurements. The predicted discharge kinetics are consistent with CFx operations. Finally, we predict Li/CFx rechargeability under the application of high potentials, along a charging pathway different from that of discharge. Our work represents a general, quasi-kinetic framework to understand the discharge of conversion cathodes, circumventing the widely used phase diagram approach which most likely does not apply to Li/CFx because equilibrium conditions are not attained in this system.
△ Less
Submitted 2 July, 2021;
originally announced July 2021.