Perspective: Challenges and opportunities for high-quality battery production at scale
Authors:
Peter M. Attia,
Eric Moch,
Patrick K. Herring
Abstract:
As the impacts of climate change become increasingly apparent, the need for widespread electrification is now internationally recognized. As a result, global battery production is set to dramatically expand over the next decade. Unfortunately, however, batteries are both immensely difficult to produce at the gigawatt-hour scale and inordinately sensitive to minor manufacturing variation. As a resu…
▽ More
As the impacts of climate change become increasingly apparent, the need for widespread electrification is now internationally recognized. As a result, global battery production is set to dramatically expand over the next decade. Unfortunately, however, batteries are both immensely difficult to produce at the gigawatt-hour scale and inordinately sensitive to minor manufacturing variation. As a result, the battery industry has already experienced a number of both highly-visible safety incidents and under-the-radar reliability issues -- a trend that will only worsen if left unaddressed. In this perspective, we highlight both the challenges and opportunities to enable battery quality at scale. We first describe the interplay between various battery failure modes and their numerous root causes. We then discuss the tensions at play to manage and improve battery quality during cell production. We hope our perspective brings greater visibility to the battery quality challenge to enable safe global electrification.
△ Less
Submitted 8 July, 2024; v1 submitted 1 March, 2024;
originally announced March 2024.
-
"Knees" in lithium-ion battery aging trajectories
Authors:
Peter M. Attia,
Alexander Bills,
Ferran Brosa Planella,
Philipp Dechent,
Gonçalo dos Reis,
Matthieu Dubarry,
Paul Gasper,
Richard Gilchrist,
Samuel Greenbank,
David Howey,
Ouyang Liu,
Edwin Khoo,
Yuliya Preger,
Abhishek Soni,
Shashank Sripad,
Anna G. Stefanopoulou,
Valentin Sulzer
Abstract:
Lithium-ion batteries can last many years but sometimes exhibit rapid, nonlinear degradation that severely limits battery lifetime. In this work, we review prior work on "knees" in lithium-ion battery aging trajectories. We first review definitions for knees and three classes of "internal state trajectories" (termed snowball, hidden, and threshold trajectories) that can cause a knee. We then discu…
▽ More
Lithium-ion batteries can last many years but sometimes exhibit rapid, nonlinear degradation that severely limits battery lifetime. In this work, we review prior work on "knees" in lithium-ion battery aging trajectories. We first review definitions for knees and three classes of "internal state trajectories" (termed snowball, hidden, and threshold trajectories) that can cause a knee. We then discuss six knee "pathways", including lithium plating, electrode saturation, resistance growth, electrolyte and additive depletion, percolation-limited connectivity, and mechanical deformation -- some of which have internal state trajectories with signals that are electrochemically undetectable. We also identify key design and usage sensitivities for knees. Finally, we discuss challenges and opportunities for knee modeling and prediction. Our findings illustrate the complexity and subtlety of lithium-ion battery degradation and can aid both academic and industrial efforts to improve battery lifetime.
△ Less
Submitted 8 January, 2022;
originally announced January 2022.
-
Electrochemical kinetics of SEI growth on carbon black, II: Modeling
Authors:
Supratim Das,
Peter M. Attia,
William C. Chueh,
Martin Z. Bazant
Abstract:
Mathematical models of capacity fade can reduce the time and cost of lithium-ion battery development and deployment, and growth of the solid-electrolyte interphase (SEI) is a major source of capacity fade. Experiments in Part I reveal nonlinear voltage dependence and strong charge-discharge asymmetry in SEI growth on carbon black negative electrodes, which is not captured by previous models. Here,…
▽ More
Mathematical models of capacity fade can reduce the time and cost of lithium-ion battery development and deployment, and growth of the solid-electrolyte interphase (SEI) is a major source of capacity fade. Experiments in Part I reveal nonlinear voltage dependence and strong charge-discharge asymmetry in SEI growth on carbon black negative electrodes, which is not captured by previous models. Here, we present a theoretical model for the electrochemical kinetics of SEI growth coupled to lithium intercalation, which accurately predicts experimental results with few adjustable parameters. The key hypothesis is that the initial SEI is a mixed ion-electron conductor, and its electronic conductivity varies approximately with the square of the local lithium concentration, consistent with hopping conduction of electrons along percolating networks. By including a lithium-ion concentration dependence for the electronic conductivity in the SEI, the bulk SEI thus modulates the overpotential and exchange current of the electrolyte reduction reaction. As a result, SEI growth is promoted during lithiation but suppressed during delithiation. This new insight establishes the fundamental electrochemistry of SEI growth kinetics. Our model improves upon existing models by introducing the effects of electrochemical SEI growth and its dependence on potential, current magnitude, and current direction in predicting capacity fade.
△ Less
Submitted 4 January, 2019;
originally announced January 2019.
-
Electrochemical kinetics of SEI growth on carbon black, I: Experiments
Authors:
Peter M. Attia,
Supratim Das,
Stephen J. Harris,
Martin Z. Bazant,
William C. Chueh
Abstract:
Growth of the solid electrolyte interphase (SEI) is a primary driver of capacity fade in lithium-ion batteries. Despite its importance to this device and intense research interest, the fundamental mechanisms underpinning SEI growth remain unclear. In Part I of this work, we present an electroanalytical method to measure the dependence of SEI growth on potential, current magnitude, and current dire…
▽ More
Growth of the solid electrolyte interphase (SEI) is a primary driver of capacity fade in lithium-ion batteries. Despite its importance to this device and intense research interest, the fundamental mechanisms underpinning SEI growth remain unclear. In Part I of this work, we present an electroanalytical method to measure the dependence of SEI growth on potential, current magnitude, and current direction during galvanostatic cycling of carbon black/Li half cells. We find that SEI growth strongly depends on all three parameters; most notably, we find SEI growth rates increase with nominal C rate and are significantly higher on lithiation than on delithiation. We observe this directional effect in both galvanostatic and potentiostatic experiments and discuss hypotheses that could explain this observation. This work identifies a strong coupling between SEI growth and charge storage (e.g., intercalation and capacitance) in carbon negative electrodes.
△ Less
Submitted 14 January, 2019; v1 submitted 4 January, 2019;
originally announced January 2019.