Fabrication of bulk delta-phase Zirconium Hydride from Zircaloy-4 for use as moderators in microreactors
Authors:
D. Parkison,
M. A. Tunes,
T. J. Nizolek,
T. A. Saleh,
P. Hosemann,
C. A. Kohnert
Abstract:
The fabrication of bulk delta-phase Zirconium Hydride ($δ$-ZrH) using Zircaloy-4 as a precursor is herein reported. Characterization using electron-microscopy methods indicate that the fabricated material is of a single-phase. Sn-rich segregation zones have been observed to form as a direct result of the hydriding process. These findings experimentally validate previous \textit{ab initio} calculat…
▽ More
The fabrication of bulk delta-phase Zirconium Hydride ($δ$-ZrH) using Zircaloy-4 as a precursor is herein reported. Characterization using electron-microscopy methods indicate that the fabricated material is of a single-phase. Sn-rich segregation zones have been observed to form as a direct result of the hydriding process. These findings experimentally validate previous \textit{ab initio} calculations on the influence H incorporation in Zircaloy-4 constitutional elements such as Sn, Fe and Cr. The effect of hydriding and Sn segregation on pre-existing Zr(Fe,Cr)$_{2}$ Laves phases is also evaluated. Major implications on the development of moderators for use in microreactors within the nuclear industry are discussed.
△ Less
Submitted 3 May, 2023;
originally announced May 2023.
-
Freestanding LiPON: from Fundamental Study to Uniformly Dense Li Metal Deposition Under Zero External Pressure
Authors:
Diyi Cheng,
Thomas Wynn,
Bingyu Lu,
Maxwell Marple,
Bing Han,
Ryosuke Shimizu,
Bhagath Sreenarayanan,
Jeffery Bickel,
Peter Hosemann,
Yangyuchen Yang,
Han Nguyen,
Weikang Li,
Guomin Zhu,
Minghao Zhang,
Ying Shirley Meng
Abstract:
Lithium phosphorus oxynitride (LiPON) is a well-known amorphous thin film solid electrolyte that has been extensively studied in the last three decades. Despite the promises to pair with Li metal anode and various cathode materials, the presence of rigid substrate and LiPONs unique amorphous, air-sensitive nature set limitations to comprehensively understand its intrinsic properties for future dev…
▽ More
Lithium phosphorus oxynitride (LiPON) is a well-known amorphous thin film solid electrolyte that has been extensively studied in the last three decades. Despite the promises to pair with Li metal anode and various cathode materials, the presence of rigid substrate and LiPONs unique amorphous, air-sensitive nature set limitations to comprehensively understand its intrinsic properties for future development and applications. This work demonstrates a methodology to synthesize LiPON in a freestanding form that exhibits remarkable flexibility and a Young s modulus of ~33 GPa. Solid-state nuclear magnetic resonance (ss-NMR) and differential scanning calorimetry (DSC) results with unprecedented high signal-to-noise ratio could be obtained with such freestanding LiPON (FS-LiPON), revealing the Li-LiPON interface bonding environments quantitatively and a well-defined glass transition temperature for LiPON. Combining interfacial stress and a seeding layer, FS-LiPON demonstrates a uniform and fully dense Li metal deposition without the aid of external pressure. Such a FS-LiPON film offers new opportunities for fundamental study of LiPON material and associated interfaces, and provides perspectives for interface engineering in bulk solid-state battery.
△ Less
Submitted 11 April, 2023; v1 submitted 8 August, 2022;
originally announced August 2022.
-
Volume 78, 1 October 2014, Pages 56-64
Authors:
A. Lupinacci,
J. Kacher,
A. A. Shapiro,
P. Hosemann,
A. M. Minor
Abstract:
Characterizing plasticity mechanisms below the ductile-to-brittle transition temperature is traditionally difficult to accomplish in asystematic fashion. Here, we use a new experimental setup to perform in situ cryogenic mechanical testing of pure Sn micropillars at room temperature and at 142°C. Subsequent electron microscopy characterization of the micropillars shows a clear difference in the de…
▽ More
Characterizing plasticity mechanisms below the ductile-to-brittle transition temperature is traditionally difficult to accomplish in asystematic fashion. Here, we use a new experimental setup to perform in situ cryogenic mechanical testing of pure Sn micropillars at room temperature and at 142°C. Subsequent electron microscopy characterization of the micropillars shows a clear difference in the deformation mechanisms at room temperature and at cryogenic temperatures. At room temperature, the Sn micropillars deformed through dislocation plasticity, while at142°C they exhibited both higher strength and deformation twinning. Two different orientations were tested, a symmetric (100) orientation and a non-symmetric (451) orientation. The deformation mechanisms were found to be the same for both orientations
△ Less
Submitted 1 April, 2021;
originally announced April 2021.
-
Compositionally Graded SS316 to C300 Maraging Steel using Additive Manufacturing
Authors:
A. Ben-Artzy,
A. Reichardt,
J-P. Borgonia,
R. P. Dillon,
B. McEnerney,
A. A. Shapiro,
P. Hosemann
Abstract:
Joining of dissimilar metals is required for numerous applications in industries such as chemical, energy and automotive. It is challenging due to differences in melting point, density, and thermal expansion of the metals being joined. Common welding techniques involve limiting melting and solidification to a narrow area leading to high thermal stresses and potentially brittle intermetallic phases…
▽ More
Joining of dissimilar metals is required for numerous applications in industries such as chemical, energy and automotive. It is challenging due to differences in melting point, density, and thermal expansion of the metals being joined. Common welding techniques involve limiting melting and solidification to a narrow area leading to high thermal stresses and potentially brittle intermetallic phases. Furthermore, the geometric complexity of these welded joints can be rather limited. Additive Manufacturing (AM) presents new techniques for joining of dissimilar metals. One of the emerging methods is the building of functionally graded parts using Directed Energy Deposition (DED) to spatially vary composition. In this paper, a SS316L and C300 maraging steel couple were joined by DED and heat treated. 13 discrete composition layers were selected using metallurgical considerations, in order to ensure a smooth transition in properties and microstructure. The mechanical properties of the as-built joints were found to be similar to the SS part and no intermetallic phases were found in the interface.
△ Less
Submitted 20 January, 2021;
originally announced January 2021.
-
Quantifying residual stress in Helium implanted surfaces and its implication for blistering
Authors:
P. Hosemann,
M. Sebastiani,
M. Z. Mughal,
X. Huang,
A. Scott,
M. Balooch
Abstract:
Helium implantation in surfaces is of interest for plasma facing materials and other nuclear applications. Vanadium as both a representative bcc material and a material relevant for fusion applications is implanted using a Helium ion beam microscope, and the resulting swelling and nanomechanical properties are quantified. These values are put in correlation to data obtained from micro residual str…
▽ More
Helium implantation in surfaces is of interest for plasma facing materials and other nuclear applications. Vanadium as both a representative bcc material and a material relevant for fusion applications is implanted using a Helium ion beam microscope, and the resulting swelling and nanomechanical properties are quantified. These values are put in correlation to data obtained from micro residual stress measurements using a focused ion beam based ring-core technique. We found that the swelling measured is similar to literature values. Further we are able to measure the surface stress caused by the implantation and find it approaches the yield strength of the material at blistering doses. The simple calculations performed in the present work, along with several geometrical considerations deduced from experimental results confirm the driving force for blister formation comes from bulging resulting mainly from gas pressure buildup, rather than solely stress induced buckling.
△ Less
Submitted 17 January, 2021;
originally announced January 2021.
-
Electrical properties of thermal oxide scales on pure iron in liquid lead-bismuth eutectic
Authors:
Jie Qiu,
Junsoo Han,
Ryan Schoell,
Miroslav Popovic,
Elmira Ghanbari,
Djamel Kaoumi,
John R Scully,
Digby D Macdonald,
Peter Hosemann
Abstract:
The impedance behavior of pre-oxidized iron in liquid lead-bismuth eutectic (LBE) at 200 oC is studied using electrochemical impedance spectroscopy. The structures and resistance of oxide grown on iron oxidized in air at different temperatures and durations are compared. The results show that the resistance of the oxide film increases with increasing oxidizing temperature, due to the formation of…
▽ More
The impedance behavior of pre-oxidized iron in liquid lead-bismuth eutectic (LBE) at 200 oC is studied using electrochemical impedance spectroscopy. The structures and resistance of oxide grown on iron oxidized in air at different temperatures and durations are compared. The results show that the resistance of the oxide film increases with increasing oxidizing temperature, due to the formation of a thicker scale and fewer defects. At the same temperature (600 oC), increasing the oxidation time can also reduce the defect concentration in the oxide film and improve the impedance of the oxide scale in LBE.
△ Less
Submitted 11 October, 2020;
originally announced October 2020.
-
Impact of interfaces on the radiation response and underlying defect recovery mechanisms in nanostructured Cu-Fe-Ag
Authors:
Michael Wurmshuber,
David Frazer,
Andrea Bachmaier,
Yongqiang Wang,
Peter Hosemann,
Daniel Kiener
Abstract:
Newest developments in nuclear fission and fusion technology as well as planned long-distance space missions demand novel materials to withstand harsh, irradiative environments. Radiation-induced hardening and embrittlement are a concern that can lead to failure of materials deployed in these applications. Here the underlying mechanisms are accommodation and clustering of lattice defects created b…
▽ More
Newest developments in nuclear fission and fusion technology as well as planned long-distance space missions demand novel materials to withstand harsh, irradiative environments. Radiation-induced hardening and embrittlement are a concern that can lead to failure of materials deployed in these applications. Here the underlying mechanisms are accommodation and clustering of lattice defects created by the incident radiation particles. Interfaces, such as free surfaces, phase and grain boundaries, are known for trapping and annihilating defects and therefore preventing these radiation-induced defects from forming clusters. In this work, differently structured nanocomposite materials based on Cu-Fe-Ag were fabricated using a novel solid-state route, combining severe plastic deformation with thermal and electrochemical treatments. The influence of different interface types and spacings on radiation effects in these materials was investigated using nanoindentation. Interface-rich bulk nanocomposites showed a slight decrease in hardness after irradiation, whereas the properties of a nanoporous material remain mostly unchanged. An explanation for this different material behavior and its link to recovery mechanisms at interfaces is attempted in this work, paving a concept towards radiation resistant materials.
△ Less
Submitted 4 September, 2020;
originally announced September 2020.
-
Atom probe characterisation of segregation driven Cu and Mn-Ni-Si co-precipitation in neutron irradiated T91 tempered-martensitic steel
Authors:
T. P. Davis,
M. A. Auger,
N. Almirall,
P. Hosemann,
G. R. Odette,
P. A. J. Bagot,
M. P. Moody,
D. E. J. Armstrong
Abstract:
The T91 grade and similar 9Cr tempered-martensitic steels (also known as ferritic-martensitic) are leading candidate structural alloys for fast fission nuclear and fusion power reactors. At low temperatures (300 to 400 $^\circ$C) neutron irradiation hardens and embrittles these steels, therefore it is important to investigate the origin of this mode of life limiting property degradation. T91 steel…
▽ More
The T91 grade and similar 9Cr tempered-martensitic steels (also known as ferritic-martensitic) are leading candidate structural alloys for fast fission nuclear and fusion power reactors. At low temperatures (300 to 400 $^\circ$C) neutron irradiation hardens and embrittles these steels, therefore it is important to investigate the origin of this mode of life limiting property degradation. T91 steel specimens were separately neutron irradiated to 2.14 dpa at 327 $^\circ$C and 8.82 dpa at 377 $^\circ$C in the Idaho National Laboratory Advanced Test Reactor. Atom probe tomography was used to investigate the segregation driven formation of Mn-Ni-Si-rich (MNSPs) and Cu-rich (CRP) co-precipitates. The precipitates increase in size and, slightly, in volume fraction at the higher irradiation temperature and dose, while their corresponding compositions were very similar, falling near the Si(Mn,Ni) phase field in the Mn-Ni-Si projection of the Fe-based quaternary phase diagram. While the structure of the precipitates has not been characterized, this composition range is distinctly different than that of the typically cited G-phase. The precipitates are composed of CRP with MNSP appendages. Such features are often observed in neutron irradiated reactor pressure vessel (RPV) steels. However, the Si, Ni, Mn, P and Cu solutes concentrations are lower in the T91 than in typical RPV steels. Thus, in T91 precipitation primarily takes place in solute segregated regions of line and loop dislocations. These results are consistent with the model for radiation induced segregation driven precipitation of MNSPs proposed by Ke et al. Cr-rich alpha prime ($α$') phase formation was not observed.
△ Less
Submitted 21 July, 2020;
originally announced July 2020.
-
Chemical manipulation of hydrogen induced high p-type and n-type conductivity in Ga2O3
Authors:
Md Minhazul Islam,
Maciej Oskar Liedke,
David Winarski,
Maik Butterling,
Andreas Wagner,
Peter Hosemann,
Yongqiang Wang,
Blas Uberuaga,
Farida A. Selim
Abstract:
Advancement of optoelectronic and high-power devices is tied to the development of wide band gap materials with excellent transport properties. However, bipolar doping (n-type and p-type doping) and realizing high carrier density while maintaining good mobility have been big challenges in wide band gap materials. Here P-type and n-type conductivity was introduced in beta-Ga2O3, an ultra-wide band…
▽ More
Advancement of optoelectronic and high-power devices is tied to the development of wide band gap materials with excellent transport properties. However, bipolar doping (n-type and p-type doping) and realizing high carrier density while maintaining good mobility have been big challenges in wide band gap materials. Here P-type and n-type conductivity was introduced in beta-Ga2O3, an ultra-wide band gap oxide, by controlling hydrogen incorporation in the lattice without further doping. Hydrogen induced a 9-order of magnitude increase of n-type conductivity with donor ionization energy of 20 meV and resistivity of 10-4 Ohm.cm. The conductivity was switched to p-type with acceptor ionization energy of 42 meV by altering hydrogen incorporation in the lattice. Density functional theory calculations were used to examine hydrogen location in the Ga2O3 lattice and identified a new donor type as the source of this remarkable n-type conductivity. Positron annihilation spectroscopy confirmed this finding and the interpretation of the results. This work illustrates a new approach that allows a tunable and reversible way of modifying the conductivity of semiconductors and it is expected to have profound implications on semiconductor field. At the same time it demonstrates for the first time p-type and remarkable n-type conductivity in Ga2O3 which should usher in the development of Ga2O3 devices and advance optoelectronics and high-power devices
△ Less
Submitted 6 November, 2019;
originally announced November 2019.
-
Key mechanistic features of swelling and blistering of helium-ion-irradiated tungsten
Authors:
Frances I. Allen,
Peter Hosemann,
Mehdi Balooch
Abstract:
Helium-ion-induced swelling and blistering of single-crystal tungsten is investigated using a Helium Ion Microscope for site-specific dose-controlled irradiation (at 25 keV) with analysis by Helium Ion Microscopy, Atomic Force Microscopy and Transmission Electron Microscopy (cross-sectioning by Focused Ion Beam milling). Our measurements show that the blister cavity forms at the depth of the heliu…
▽ More
Helium-ion-induced swelling and blistering of single-crystal tungsten is investigated using a Helium Ion Microscope for site-specific dose-controlled irradiation (at 25 keV) with analysis by Helium Ion Microscopy, Atomic Force Microscopy and Transmission Electron Microscopy (cross-sectioning by Focused Ion Beam milling). Our measurements show that the blister cavity forms at the depth of the helium peak and that nanobubbles coalesce to form nanocracks within the envelope of the ion stopping range, causing swelling of the blister shell. These results provide the first direct experimental evidence for the interbubble fracture mechanism proposed in the framework of the gas pressure model for blister formation.
△ Less
Submitted 4 September, 2019;
originally announced September 2019.
-
Effect of strain and temperature on the threshold displacement energy in body-centered cubic iron
Authors:
Benjamin Beeler,
Mark Asta,
Peter Hosemann,
Niels Gronbech-Jensen
Abstract:
The threshold displacement energy (TDE) is the minimum amount of kinetic energy required to displace an atom from its lattice site. The magnitude of the TDE displays significant variance as a function of the crystallographic direction, system temperature and applied strain, among a variety of other factors. It is critically important to determine an accurate value of the TDE in order to calculate…
▽ More
The threshold displacement energy (TDE) is the minimum amount of kinetic energy required to displace an atom from its lattice site. The magnitude of the TDE displays significant variance as a function of the crystallographic direction, system temperature and applied strain, among a variety of other factors. It is critically important to determine an accurate value of the TDE in order to calculate the total number of displacements due to a given irradiation condition, and thus to understand the materials response to irradiation. In this study, molecular dynamics simulations have been performed to calculate the threshold displacement energy in body-centered cubic iron as a function of strain and temperature. With applied strain, a decrease of the TDE of up to approximately 14 eV was observed. A temperature increase from 300 K to 500 K can result in an increase of the TDE of up to approximately 9 eV.
△ Less
Submitted 6 April, 2016;
originally announced April 2016.
-
Effects of applied strain on radiation damage generation in body-centered cubic iron
Authors:
Benjamin Beeler,
Mark Asta,
Peter Hosemann,
Niels Grønbech-Jensen
Abstract:
Radiation damage in body-centered cubic (BCC) Fe has been extensively studied by computer simulations to quantify effects of temperature, impinging particle energy, and the presence of extrinsic particles. However, limited investigation has been conducted into the effects of mechanical stresses and strain. In a reactor environment, structural materials are often mechanically strained, and an expan…
▽ More
Radiation damage in body-centered cubic (BCC) Fe has been extensively studied by computer simulations to quantify effects of temperature, impinging particle energy, and the presence of extrinsic particles. However, limited investigation has been conducted into the effects of mechanical stresses and strain. In a reactor environment, structural materials are often mechanically strained, and an expanded understanding of how this strain affects the generation of defects may be important for predicting microstructural evolution and damage accumulation under such conditions. In this study, we have performed molecular dynamics simulations in which various types of homogeneous strains are applied to BCC Fe and the effect on defect generation is examined. It is found that volume-conserving shear strains yield no statistically significant variations in the stable number of defects created via cascades in BCC Fe. However, strains that result in volume changes are found to produce significant effects on defect generation.
△ Less
Submitted 28 December, 2014; v1 submitted 11 September, 2014;
originally announced September 2014.
-
Accessing defect dynamics using intense, nanosecond pulsed ion beams
Authors:
A. Persaud,
J. J. Barnard,
H. Guo,
P. Hosemann,
S. Lidia,
A. M. Minor,
P. A. Seidl,
T. Schenkel
Abstract:
Gaining in-situ access to relaxation dynamics of radiation induced defects will lead to a better understanding of materials and is important for the verification of theoretical models and simulations. We show preliminary results from experiments at the new Neutralized Drift Compression Experiment (NDCX-II) at Lawrence Berkeley National Laboratory that will enable in-situ access to defect dynamics…
▽ More
Gaining in-situ access to relaxation dynamics of radiation induced defects will lead to a better understanding of materials and is important for the verification of theoretical models and simulations. We show preliminary results from experiments at the new Neutralized Drift Compression Experiment (NDCX-II) at Lawrence Berkeley National Laboratory that will enable in-situ access to defect dynamics through pump-probe experiments. Here, the unique capabilities of the NDCX-II accelerator to generate intense, nanosecond pulsed ion beams are utilized. Preliminary data of channeling experiments using lithium and potassium ions and silicon membranes are shown. We compare these data to simulation results using Crystal Trim. Furthermore, we discuss the improvements to the accelerator to higher performance levels and the new diagnostics tools that are being incorporated.
△ Less
Submitted 8 September, 2014;
originally announced September 2014.
-
Towards pump-probe experiments of defect dynamics with short ion beam pulses
Authors:
T. Schenkel,
S. M. Lidia,
C. D. Weis,
W. L. Waldron,
J. Schwartz,
A. M. Minor,
P. Hosemann,
J. W. Kwan
Abstract:
A novel, induction type linear accelerator, the Neutralized Drift Compression eXperiment (NDCX-II), is currently being commissioned at Berkeley Lab. This accelerator is designed to deliver intense (up to 3x1011 ions/pulse), 0.6 to ~600 ns duration pulses of 0.13 to 1.2 MeV lithium ions at a rate of about 2 pulses per minute onto 1 to 10 mm scale target areas. When focused to mm-diameter spots, the…
▽ More
A novel, induction type linear accelerator, the Neutralized Drift Compression eXperiment (NDCX-II), is currently being commissioned at Berkeley Lab. This accelerator is designed to deliver intense (up to 3x1011 ions/pulse), 0.6 to ~600 ns duration pulses of 0.13 to 1.2 MeV lithium ions at a rate of about 2 pulses per minute onto 1 to 10 mm scale target areas. When focused to mm-diameter spots, the beam is predicted to volumetrically heat micrometer thick foils to temperatures of ~30,000 K. At lower beam power densities, the short excitation pulse with tunable intensity and time profile enables pump-probe type studies of defect dynamics in a broad range of materials. We briefly describe the accelerator concept and design, present results from beam pulse shaping experiments and discuss examples of pump-probe type studies of defect dynamics following irradiation of materials with intense, short ion beam pulses from NDCX-II.
△ Less
Submitted 23 April, 2013; v1 submitted 27 November, 2012;