Magnetic properties of Ge, Re and Cr substituted Fe$_5$SiB$_2$
Authors:
M. Casadei,
M. M. Isah,
R. Cabassi,
G. Trevisi,
S. Fabbrici,
M. Belli,
C. de Julián Fernández,
G. Allodi,
V. Fournée,
S. Sanna,
F. Albertini
Abstract:
One of the possible approaches to decrease the demand for critical elements such as rare earths is to develop new sustainable magnets. Iron-based materials are suitable for gap magnets applications since iron is the most abundant ferromagnetic element on Earth. Fe$_5$SiB$_2$ is a candidate as gap magnet thanks to its high Curie temperature (T$_{\text{C}} \sim$ 800 K) and saturation magnetization (…
▽ More
One of the possible approaches to decrease the demand for critical elements such as rare earths is to develop new sustainable magnets. Iron-based materials are suitable for gap magnets applications since iron is the most abundant ferromagnetic element on Earth. Fe$_5$SiB$_2$ is a candidate as gap magnet thanks to its high Curie temperature (T$_{\text{C}} \sim$ 800 K) and saturation magnetization (M$_{\text{S}}\sim$ 140 Am$^2$kg$^{-1}$). However its anisotropy field is too low for applications (H$_{\text{A}} \sim$ 0.8 T). In order to increase the anisotropy value, we synthesized a series of Ge, Re and Cr substituted Fe$_5$SiB$_2$ samples and studied their magnetic properties. They all crystallize in the Cr$_5$B$_3$-type tetragonal structure with the $I4/mcm$ space group. Curie temperature (T$_{\text{C}}$ = 803 K) and saturation magnetization (M$_{\text{S}}$ = 138 Am$^2$kg$^{-1}$) are slightly decreased by elemental substitution with Re having the largest effect. Despite being reduced, T$_{\text{C}}$ and M$_{\text{S}}$ still maintain significant values (T$_{\text{C}}>$ 750 K and M$_{\text{S}}$ = 118 Am$^2$kg$^{-1}$). The room temperature anisotropy field has been measured by Singular Point Detection (SPD) and increases by about 15% upon Re substitution, reaching 0.92 T for Fe$_{4.75}$Re$_{0.25}$SiB$_2$. We have also used Nuclear Magnetic Resonance and SPD measurements to study the spin reorientation transition which takes place at 172 K and we have found that it is partially suppressed by substitution of Ge from 172 K to 140 K and completely suppressed upon Cr and Re substitution.
△ Less
Submitted 2 January, 2025;
originally announced January 2025.
-
Dense strontium hexaferrite-based permanent magnet composites assisted by cold sintering process
Authors:
Eduardo García-Martín,
Cecilia Granados-Miralles,
Sandra Ruiz-Gómez,
Lucas Pérez,
Adolfo del Campo,
Jesús Carlos Guzmán-Mínguez,
César de Julián Fernández,
Adrián Quesada,
José F. Fernández,
Aida Serrano
Abstract:
The use of rare-earth-based permanent magnets is one of the critical points for the development of the current technology. On the one hand, industry of the rare-earths is highly polluting due to the negative environmental impact of their extraction and, on the other hand, the sector is potentially dependent on China. Therefore, investigation is required both in the development of rare-earth-free p…
▽ More
The use of rare-earth-based permanent magnets is one of the critical points for the development of the current technology. On the one hand, industry of the rare-earths is highly polluting due to the negative environmental impact of their extraction and, on the other hand, the sector is potentially dependent on China. Therefore, investigation is required both in the development of rare-earth-free permanent magnets and in sintering processes that enable their greener fabrication with attractive magnetic properties at a more competitive price. This work presents the use of a cold sintering process (CSP) followed by a post-annealing at 1100 °C as a new way to sinter composite permanent magnets based on strontium ferrite (SFO). Composites that incorporate a percentage < 10% of an additional magnetic phase have been prepared and the morphological, structural and magnetic properties have been evaluated after each stage of the process. CSP induces a phase transformation of SFO in the composites, which is partially recovered by the post-thermal treatment improving the relative density to 92% and the magnetic response of the final magnets with a coercivity of up to 3.0 kOe. Control of the magnetic properties is possible through the composition and the grain size in the sintered magnets. These attractive results show the potential of the sintering approach as an alternative to develop modern rare-earth-free composite permanent magnets.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
FeCo Nanowire-Strontium Ferrite Powder Composites for Permanent Magnets with High-Energy Products
Authors:
J. C. Guzmán-Mínguez,
S. Ruiz-Gómez,
L. M. Vicente-Arche,
C. Granados-Miralles,
C. Fernández-González,
F. Mompeán,
M. García-Hernández,
S. Erohkin,
D. Berkov,
D. Mishra,
C. de Julián Fernández,
J. F. Fernández,
L. Pérez,
A. Quesada
Abstract:
Due to the issues associated with rare-earth elements, there arises a strong need for magnets with properties between those of ferrites and rare-earth magnets that could substitute the latter in selected applications. Here, we produce a high remanent magnetization composite bonded magnet by mixing FeCo nanowire powders with hexaferrite particles. In the first step, metallic nanowires with diameter…
▽ More
Due to the issues associated with rare-earth elements, there arises a strong need for magnets with properties between those of ferrites and rare-earth magnets that could substitute the latter in selected applications. Here, we produce a high remanent magnetization composite bonded magnet by mixing FeCo nanowire powders with hexaferrite particles. In the first step, metallic nanowires with diameters between 30 and 100 nm and length of at least 2 μm are fabricated by electrodeposition. The oriented as-synthesized nanowires show remanence ratios above 0.76 and coercivities above 199 kA/m and resist core oxidation up to 300 °C due to the existence of a > 8 nm thin oxide passivating shell. In the second step, a composite powder is fabricated by mixing the nanowires with hexaferrite particles. After the optimal nanowire diameter and composite composition are selected, a bonded magnet is produced. The resulting magnet presents a 20% increase in remanence and an enhancement of the energy product of 48% with respect to a pure hexaferrite (strontium ferrite) magnet. These results put nanowire-ferrite composites at the forefront as candidate materials for alternative magnets for substitution of rare earths in applications that operate with moderate magnet performance.
△ Less
Submitted 24 September, 2023;
originally announced September 2023.
-
Remanence Increase in SrFe$_{12}$O$_{19}$/Fe Exchange-Decoupled Hard-Soft Composite Magnets Owing to Dipolar Interactions
Authors:
Jesús Carlos Guzmán-Mínguez,
Cecilia Granados-Miralles,
Patrick Kuntschke,
César de Julián Fernández,
Sergey Erokhin,
Dmitry Berkov,
Thomas Schliesch,
Jose Francisco Fernández,
Adrián Quesada
Abstract:
In the search for improved permanent magnets, fueled by the geostrategic and environmental issues associated with rare-earth-based magnets, magnetically hard (high anisotropy)-soft (high magnetization) composite magnets hold promise as alternative magnets that could replace modern permanent magnets, such as rare-earth-based and ceramic magnets, in certain applications. However, so far, the magneti…
▽ More
In the search for improved permanent magnets, fueled by the geostrategic and environmental issues associated with rare-earth-based magnets, magnetically hard (high anisotropy)-soft (high magnetization) composite magnets hold promise as alternative magnets that could replace modern permanent magnets, such as rare-earth-based and ceramic magnets, in certain applications. However, so far, the magnetic properties reported for hard-soft composites have been underwhelming. Here, an attempt to further understand the correlation between magnetic and microstructural properties in strontium ferrite-based composites, hard SrFe$_{12}$O$_{19}$ (SFO) ceramics with different contents of Fe particles as soft phase, both in powder and in dense injection molded magnets, is presented. In addition, the influence of soft phase particle dimension, in the nano- and micron-sized regimes, on these properties is studied. While Fe and SFO are not exchange-coupled in our magnets, a remanence that is higher than expected is measured. In fact, in composite injection molded anisotropic (magnetically oriented) magnets, remanence is improved by 2.4% with respect to a pure ferrite identical magnet. The analysis of the experimental results in combination with micromagnetic simulations allows us to establish that the type of interaction between hard and soft phases is of a dipolar nature, and is responsible for the alignment of a fraction of the soft spins with the magnetization of the hard. The mechanism unraveled in this work has implications for the development of novel hard-soft permanent magnets.
△ Less
Submitted 19 September, 2023;
originally announced September 2023.