XPS analysis of molecular contamination and sp2 amorphous carbon on oxidized (100) diamond
Authors:
Ricardo Vidrio,
Daniel Vincent,
Benjamin Bachman,
Cesar Saucedo,
Maryam Zahedian,
Zihong Xu,
Junyu Lai,
Timothy A. Grotjohn,
Shimon Kolkowitz,
Jung-Hun Seo,
Robert J. Hamers,
Keith G. Ray,
Zhenqiang Ma,
Jennifer T. Choy
Abstract:
The efficacy of oxygen (O) surface terminations on diamond is an important factor for the performance and stability for diamond-based quantum sensors and electronics. Given the wide breadth of O-termination techniques, it can be difficult to discern which method would yield the highest and most consistent O coverage. Furthermore, the interpretation of surface characterization techniques is complic…
▽ More
The efficacy of oxygen (O) surface terminations on diamond is an important factor for the performance and stability for diamond-based quantum sensors and electronics. Given the wide breadth of O-termination techniques, it can be difficult to discern which method would yield the highest and most consistent O coverage. Furthermore, the interpretation of surface characterization techniques is complicated by surface morphology and purity, which if not accounted for will yield inconsistent determination of the oxygen coverage. We present a comprehensive approach to consistently prepare and analyze oxygen termination of surfaces on (100) single-crystalline diamond. We report on X-ray Photoelectron Spectroscopy (XPS) characterization of diamond surfaces treated with six oxidation methods that include various wet chemical oxidation techniques, photochemical oxidation with UV illumination, and steam oxidation using atomic layer deposition (ALD). Our analysis entails a rigorous XPS peak-fitting procedure for measuring the functionalization of O-terminated diamond. The findings herein have provided molecular-level insights on oxidized surfaces in (100) diamond, including the demonstration of clear correlation between the measured oxygen atomic percentage and the presence of molecular contaminants containing nitrogen, silicon, and sulfur. We also provide a comparison of the sp2 carbon content with the O1s atomic percentage and discern a correlation with the diamond samples treated with dry oxidation which eventually tapers off at a max O1s atomic percentage value of 7.09 +/- 0.40%. Given these results, we conclude that the dry oxidation methods yield some of the highest oxygen amounts, with the ALD water vapor technique proving to be the cleanest technique out of all the oxidation methods explored in this work.
△ Less
Submitted 8 May, 2024; v1 submitted 5 April, 2023;
originally announced April 2023.
The Effects of Boron Doping on the Bulk and Surface Acoustic Phonons in Single-Crystal Diamond
Authors:
Erick Guzman,
Fariborz Kargar,
Frank Angeles,
Reza Vatan Meidanshahi,
Timothy A. Grotjohn,
Aaron Hardy,
Matthias Muehle,
Richard B. Wilson,
Stephen Goodnik,
Alexander A. Balandin
Abstract:
We report the results of the investigation of bulk and surface acoustic phonons in the undoped and boron-doped single-crystal diamond films using the Brillouin-Mandelstam light scattering spectroscopy. The evolution of the optical phonons in the same set of samples was monitored with Raman spectroscopy. It was found that the frequency and the group velocity of acoustic phonons decrease non-monoton…
▽ More
We report the results of the investigation of bulk and surface acoustic phonons in the undoped and boron-doped single-crystal diamond films using the Brillouin-Mandelstam light scattering spectroscopy. The evolution of the optical phonons in the same set of samples was monitored with Raman spectroscopy. It was found that the frequency and the group velocity of acoustic phonons decrease non-monotonically with the increasing boron doping concentration, revealing pronounced phonon softening. The change in the velocity of the shear horizontal and the high-frequency pseudo-longitudinal acoustic phonons in the degenerately doped diamond, as compared to the undoped diamond, was as large as ~15% and ~12%, respectively. As a result of boron doping, the velocity of the bulk longitudinal and transverse acoustic phonons decreased correspondingly. The frequency of the optical phonons was unaffected at low boron concentration but experienced a strong decrease at the high doping level. The density-functional-theory calculations of the phonon band structure for the pristine and highly-doped sample confirm the phonon softening as a result of boron doping in diamond. The obtained results have important implications for thermal transport in heavily doped diamond, which is a promising material for ultra-wide-band-gap electronics.
△ Less
Submitted 23 June, 2022;
originally announced June 2022.